发明名称 Hydrogen Storing Alloy
摘要 A hydrogen storing alloy containing only a few impurities leading to a short circuit where the yield can be maintained even when the alloy is subjected to magnetic separation treatment. A hydrogen storing alloy includes a matrix phase having an AB5 type crystal structure, the alloy having a misch metal (referred to as “Mm”) in an A-site in an ABx composition and having any one or at least one of Ni, Al, Mn, and Co in a B-site in the ABx composition, wherein the ratio (referred to as “ABx”) of the total number of moles of elements comprising the B site to the total number of moles of elements comprising the A site is 5.00<ABx≦5.40; the content of Co is more than 0.0 mol % and less than 0.7 mol %; and residual magnetization is more than 0 emu/g and 0.020 emu/g or less.
申请公布号 US2016298214(A1) 申请公布日期 2016.10.13
申请号 US201515100351 申请日期 2015.03.25
申请人 MITSUI MINING & SMELTING CO., LTD. 发明人 Kikugawa Shingo;Miyanohara Keisuke;Hata Yoshimi
分类号 C22C19/00;C22F1/10;C22C1/02;H01M10/04;B22D21/00;H01M4/04;H01M4/38;H01M10/34;C22C19/03;B22D7/00 主分类号 C22C19/00
代理机构 代理人
主权项 1. A hydrogen storing alloy comprising a matrix phase having a CaCu5-type, that is, an AB5-type crystal structure, having a general formula: MmNiaMnbAlcCod, where “Mm” represents a misch metal, “a” is more than 3.8 and less than 4.7, “b” is more than 0.1 and less than 0.6, “c” is more than 0.1 and less than 0.6, and “d” is more than 0.0 and less than 0.7 or a general formula: MmNiaMnbAlcCodMe, wherein element “Mm” represents a misch metal, “M” represents at least one selected from the group consisting of Fe, Cu, V, Zn and Zr, “a” is more than 3.8 and less than 4.7, “b” is more than 0.1 and less than 0.6, “c” is more than 0.1 and less than 0.6, “d” is more than 0.0 and less than 0.7 and “e” is more than 0 and less than 0.20, wherein the ratio (referred to as “ABx”) of the total number of moles of elements comprising the B-site to the total number of moles of elements comprising the A-site is 5.00<ABx≦5.40; the ratio of the number of moles of Co to the total number of moles of elements comprising the A-site is more than 0.0 and less than 0.7; and residual magnetization is more than 0 emu/g and 0.020 emu/g or less.
地址 Tokyo JP