发明名称 ШИХТА ДЛЯ ИЗГОТОВЛЕНИЯ ОГНЕУПОРОВ
摘要 FIELD: manufacture of refractory materials of corundum composition; manufacture of articles for lining of different thermal units working at high temperatures. ^ SUBSTANCE: charge includes synthetic corundum modified with readily decomposing additive of aluminate composition (for example, aluminum nitrate, aluminum formiate, bauxite, etc.) in the amount of 1-5 mass-% and phosphate binder. Used as phosphate binder is aluminum-boro-phosphate binder at the following composition of components, mass-%: modified corundum, 90-93 and phosphate binder, 7-10. Proposed charge makes it possible to reduce its sintering temperature and porosity of articles at enhanced strength and heat resistance and additional residual change in sizes at heating (by 1-13%). ^ EFFECT: enhanced efficiency. ^ 1 tbl, 4 ex
申请公布号 RU2003122324(A) 申请公布日期 2005.01.10
申请号 RU20030122324 申请日期 2003.07.16
申请人 Ивановский государственный химико-технологический университет (RU) 发明人 Косенко Надежда Федоровна (RU);Филатова Наталь  Владимировна (RU);Шитов Владимир Александрович (RU);Морозов Борис Александрович (RU);Петров Николай Аркадьевич (RU)
分类号 C04B35/10;C04B35/622 主分类号 C04B35/10
代理机构 代理人
主权项
地址