发明名称 |
Elastomeric composition with improved thermal conductivity |
摘要 |
A rubber composition based on at least one diene elastomer, a filler that contains carbon black and an inorganic filler, and a crosslinking system, wherein the inorganic filler content is greater than or equal to 5 parts by weight per hundred parts by weight of elastomer, phr, and represents at most 50% as a weight fraction of the whole of the total filler of the composition, and wherein the carbon black includes at least one acetylene-derived carbon black, with a content of greater than 3 phr, the amount of acetylene-derived carbon black representing more than 50% of the carbon black present in the composition as a weight fraction, and wherein the composition contains a plasticizing oil or a plasticizing resin with a total content of plasticizing oil and plasticizing resin of less than 30 phr. |
申请公布号 |
US9499730(B2) |
申请公布日期 |
2016.11.22 |
申请号 |
US201314405993 |
申请日期 |
2013.06.10 |
申请人 |
COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN;MICHELIN RECHERCHE ET TECHNIQUE, S.A. |
发明人 |
Joseph, Jr. Aurelie;De Gaudemaris Benoit;Sevignon Marc |
分类号 |
C09K5/14;C08K3/00;C08K3/04;B29C43/24;B60C1/00;C08K3/36;C08K5/01;B29K9/00;B29K507/04;B29L7/00 |
主分类号 |
C09K5/14 |
代理机构 |
Dickinson Wright PLLC |
代理人 |
Dickinson Wright PLLC |
主权项 |
1. A rubber composition based on at least one diene elastomer, a filler that comprises carbon black and an inorganic filler, and a crosslinking system,
wherein the inorganic filler content is from 8 to 30 parts by weight per hundred parts by weight of elastomer, phr, and represents at most 50% as a weight fraction of the total filler of the composition wherein the carbon black comprises at least one acetylene-derived carbon black, wherein the acetylene-derived carbon black content is from 10 to 40 phr, wherein the amount of acetylene-derived carbon black represents more than 50% of the carbon black present in the composition as a weight fraction, and wherein the composition comprises a plasticizing oil, aplasticizing resin, or both, with a total content of plasticizing oil and plasticizing resin of less than 30 phr. |