发明名称 CONTINUOUS CASTING DEVICE FOR SLAB COMPRISING TITANIUM OR TITANIUM ALLOY
摘要 In the present invention the torch movement period is 20-40 seconds, with the torch movement period being the time required to move plasma torches (which heat the surface of molten metal in the casting mold) one time. The average heat input amount at multiple sites, which are obtained by dividing the initial solidification portion (which is where the molten metal makes contact with the casting mold and first solidifies) into multiple sites in the circumferential direction of the casting mold, is 1.0-2.0 MW/m2. The molten metal advection time, which is the time required for electromagnetically stirred molten metal to travel the length of the torch heating region of the surface of the molten metal in the lengthwise direction of the casting mold, is 3.5 seconds or less.
申请公布号 US2017087625(A1) 申请公布日期 2017.03.30
申请号 US201515127834 申请日期 2015.03.20
申请人 Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.) 发明人 KUROSAWA Eisuke;NAKAOKA Takehiro;OYAMA Hideto;KANAHASHI Hidetaka
分类号 B22D11/115;H05H1/44;B22D21/00;F27D27/00;B22D11/00;B22D11/041 主分类号 B22D11/115
代理机构 代理人
主权项 1. A continuous casting device for continuously casting a slab made of titanium or a titanium alloy by injecting molten metal prepared by melting titanium or a titanium alloy into a bottomless mold having a rectangular cross section and withdrawing the molten metal downward while being solidified, the device comprising: a plasma torch for heating a melt surface of the molten metal in the mold while moving over the melt surface of the molten metal in a predetermined moving pattern, the plasma torch being disposed above the mold; and an electromagnetic stirring device for stirring at least the melt surface of the molten metal by electromagnetic stirring, the electromagnetic stirring device being disposed on a side of the mold, the device having: a torch moving cycle T of 20 sec or more and 40 sec or less, the torch moving cycle T being a time required for the plasma torch to complete a single round of movement in the predetermined moving pattern and calculated by T=4W/(A·Vt), where 2W represents a length of a long side of the slab in a horizontal cross section, A represents the number of the plasma torch, and Vt represents an average moving speed of the plasma torch while moving in the predetermined moving pattern; an average heat input quantity of 1.0 MW/m2 or more and 2.0 MW/m2 or less, the average heat input quantity being obtained by dividing an initial solidification portion, where the molten metal is initially solidified upon contacting with the mold, into a plurality of portions in a peripheral direction of the mold, and calculating an average of heat input quantities to each of the portions in a length direction of the corresponding portion along the mold; and a molten metal advection time Tm of 3.5 sec or less, the molten metal advection time being calculated by Tm=L/Vm, where L represents a length of a torch heating region along a long side direction of the mold, the torch heating region being a region of the melt surface of the molten metal, which is heated by the individual plasma torch, and Vm represents an average flow rate of the molten metal while traveling the length L by electromagnetic stirring, and representing a time required for the molten metal to travel the length L of the torch heating region along the long side direction of the mold.
地址 Hyogo JP