The invention relates to a composite part, also referred to as composite below, produced from at least one part consisting of at least one polyamide molding compound that has polybutadiene copolymer additives, which are liquid at room temperature, and at least one part consisting of at least one elastomer, which can be obtained from rubber that is to be vulcanized or crosslinked with elemental sulfur, using two-component processing methods, preferably a two-component injection-molding process (2C injection molding), or the composite part is assembled from said components after the components have been processed. |