摘要 |
The present disclosure relates to a solid curable transparent rubber composition containing a styrenic block copolymer having 2 or more poly(vinyl aromatic) blocks, a curing agent and additives. Once cured, the solid curable transparent rubber composition has a haze of less than 30% and a total light transmission of more than 80%. The disclosure further relates to a cured transparent rubber composition made thereof, and a manufacturing process for the cured composition. The present disclosure also relates to an article including the rubber composition, in particular for tubes, medical stoppers, catheters, dental dams and other medical applications and artificial nipples. |
主权项 |
1. A solid curable, transparent, rubber composition that once cured has a haze of less than 30% and a total light transmission of more than 80%, both measured according to ASTM D1003-13, comprising:
Component (a): from 76 to about 100 wt. % of a styrenic block copolymer having 2 or more poly(vinyl aromatic) blocks and at least one block of polymerized conjugated diene, wherein the styrenic block copolymer has a weight average molecular weight of 150,000 to 250,000, the poly(vinyl aromatic) blocks have a weight average molecular weight ranging from 9,000 to 15,000, and the content of poly(vinyl aromatic) blocks in the styrenic block copolymer ranges from 8 to 13 wt. %, based on the total styrenic block copolymer; Components (b) and (c): from 0.05-8.0 wt. % of a curing agent, optionally with a co-agent, and Component (d): from 0.01-20 wt. % of additives that do not influence the transparency, wherein all amounts are in percentages by weight on the total composition. |