发明名称 耐熱鋼およびその製造方法
摘要 PROBLEM TO BE SOLVED: To provide a heat resistant steel that has improved long-term creep rupture life and is superior in high temperature properties and durability.SOLUTION: A heat resistant steel includes, in mass%, C: 0.05-0.2%, Si: 0.1% or less, Mn: more than 0.1% and 0.7% or less, Ni: 1% or less, Cr: 8.5% to less than 10%, Mo: 1% or less, V: 0.05-0.3%, Co: 2% or less, W: 1-5%, N: 0.01% to less than 0.014%, Nb: 0.01-0.15%, and B: 0.003-0.03%, with the balance being Fe and inevitable impurities.
申请公布号 JP5996403(B2) 申请公布日期 2016.09.21
申请号 JP20120262820 申请日期 2012.11.30
申请人 株式会社東芝 发明人 大西 春樹;山田 政之;高久 歴;久保 貴博;村田 頼治;今井 健一
分类号 C22C38/00;C21D6/00;C22C38/54;F01D5/28;F01D25/00 主分类号 C22C38/00