发明名称 FUEL CELL VEHICLE COOLANT HAVING IMPROVED STORAGE STABILITY AND METHOD FOR PRODUCING THE SAME
摘要 There are provided a stock solution composition for fuel cell vehicle coolant used by dilution with a diluent comprising water and a method for producing the same, and further a fuel cell vehicle coolant composition having improved storage stability and a method for producing the same. The present invention relates to a method for producing a stock solution composition for fuel cell vehicle coolant, wherein the stock solution composition comprises at least one ethylene glycol compound selected from the group consisting of ethylene glycol, diethylene glycol, and triethylene glycol, and is used by dilution with a diluent comprising water, and the method comprises the following steps: (a) a step of selecting as a raw material an ethylene glycol compound having an ethylene glycol monoformate content of 60 ppm or less; or (b) a step of selecting as a raw material an ethylene glycol compound, wherein a 50% by mass aqueous solution of the ethylene glycol compound has a conductivity of 4.5 μS/cm or less after heating.
申请公布号 US2016141646(A1) 申请公布日期 2016.05.19
申请号 US201514927577 申请日期 2015.10.30
申请人 TOYOTA JIDOSHA KABUSHIKI KAISHA 发明人 SUGIYAMA Yuichiro;MIYAJIMA Kazuhiro;YOSHII Youichirou;TAKAGI Nobukazu;NAKANO Tomoyuki;OTSUBO Takumi
分类号 H01M8/04;C09K5/10 主分类号 H01M8/04
代理机构 代理人
主权项 1. A method for producing a stock solution composition for fuel cell vehicle coolant, wherein the stock solution composition comprises at least one ethylene glycol compound selected from the group consisting of ethylene glycol, diethylene glycol, and triethylene glycol, and is used by dilution with a diluent comprising water, and the method comprises the following steps: (a) a step of selecting as a raw material an ethylene glycol compound having an ethylene glycol monoformate content of 60 ppm or less; or (b) a step of selecting as a raw material an ethylene glycol compound, wherein a 50% by mass aqueous solution of the ethylene glycol compound has a conductivity of 4.5 μS/cm or less after heating.
地址 Toyota-shi JP