PROBLEM TO BE SOLVED: To provide a joint member manufacturing apparatus that manufactures the joint member without causing the generation of bubbles in the adhesive and also that can quickly manufacture the joint member.SOLUTION: When a voltage impression device 21 and the faces of two members 11a, 11b that are coated with adhesive 14a, 14b, come to a position where they are facing each other in a line form, a voltage is impressed between the two members 11a, 11b and the adhesive on one side of the rectangular faces that are facing each other, is brought into contact in a line form. Then, joint member is manufactured by sliding one of the two members 11a, 11b that are brought into contact in a line form, along the bonding surface by use of a driving device 17, and superimposing the two members 11a, 11b. |