发明名称 銅合金の製造方法
摘要 <P>PROBLEM TO BE SOLVED: To provide a method for manufacturing a high-strength copper alloy containing Ti in place of a copper alloy containing Be. <P>SOLUTION: A copper alloy containing, by mass, 0.05-4% Ti and 0.01-0.7% Cr is melted at the temperature TM(&deg;C) and higher obtained from formula (1), and then, solidified to form a cast slab. In the cast slab, the area in the section orthogonal to the longitudinal direction is &ge;100 times the area in the section orthogonal to the longitudinal direction of a final product. TM=TL+20[Ti]+150[Cr]+90: (1), where in formula, TL denotes the liquidus temperature (&deg;C) obtained from specified formula, and each element symbol denotes the content (mass%) of each element. <P>COPYRIGHT: (C)2011,JPO&INPIT
申请公布号 JP5873618(B2) 申请公布日期 2016.03.01
申请号 JP20090188822 申请日期 2009.08.18
申请人 新日鐵住金株式会社 发明人 前原 泰裕
分类号 B21B3/00;C22C9/00;C22F1/00;C22F1/08 主分类号 B21B3/00
代理机构 代理人
主权项
地址