A polyester resin characterized in that the glass transition temperature is from -40 to 40°C, the number of inflection points in a temperature-deformation curve measured by a softening temperature test method by thermomechanical analysis in accordance with JIS K7196 is 2-7, and the maximum value of the inflection point temperature is 5-55°C. |