摘要 |
Injection molded articles having large, thin sections are prepared by injection molding of a composition that includes specific amounts of poly(arylene ether) and a rubber-modified polystyrene. The specific component amounts provide the composition with a shear thinning index of 6 to 17 measured at a temperature of 260 to 300° C. and shear rates of 100 and 10,000 second−1. |