发明名称 |
METHOD FOR RECOVERING CHROMITE, AND METHOD FOR WET SMELTING OF NICKEL OXIDE ORE |
摘要 |
A method for recovering chromite from ore slurry obtained by processing nickel oxide ore, the raw material, in a plant for the wet smelting of nickel oxide ore. In the method chromite is separated and recovered from an ore slurry obtained from a nickel oxide ore when nickel and cobalt are recovered from the nickel oxide ore. The method has a grain diameter separation step for separating the ore slurry on the basis of a predetermined classification point according to the difference in the grain diameter of particles contained in the supplied ore slurry and a sedimentation separation step for causing the oversized ore slurry separated in the grain diameter separation step to undergo sedimentation and concentration on the basis of a target classification point, and recovering the chromite. The coarse particle content of the oversized ore slurry separated in the grain diameter separation step is adjusted to 30-50%. |
申请公布号 |
US2015014225(A1) |
申请公布日期 |
2015.01.15 |
申请号 |
US201214384616 |
申请日期 |
2012.04.06 |
申请人 |
Mitsui Hiroyuki;Nakai Osamu;Kawasaki Hirotaka;Kobayashi Hiroshi;Higaki Tatsuya;Idegami Atsushi |
发明人 |
Mitsui Hiroyuki;Nakai Osamu;Kawasaki Hirotaka;Kobayashi Hiroshi;Higaki Tatsuya;Idegami Atsushi |
分类号 |
C22B3/22;B03B7/00 |
主分类号 |
C22B3/22 |
代理机构 |
|
代理人 |
|
主权项 |
1. A chromite recovery method for separating and recovering chromite from ore slurry produced from nickel oxide ore when recovering nickel and cobalt from the nickel oxide ore, the method comprises:
a particle diameter separation step of separating the ore slurry which has a particle size of 2 mm or less based on a predetermined classification point depending on a particle diameter difference of particles contained in the ore slurry to be supplied; and a sedimentation separation step of sedimenting and concentrating oversized ore slurry separated in the particle diameter separation step to recover the chromite, wherein a content percentage of coarse particles in the oversized ore slurry separated in the particle diameter separation step is adjusted to 30 to 50%. |
地址 |
Tokyo JP |