发明名称 FLUORORUBBER COMPOSITION
摘要 A fluororubber composition which includes a fluororubber (A) and a carbon black (B). The fluororubber (A) is a vinylidene fluoride-based fluororubber including a structural unit (VdF unit) derived from vinylidene fluoride and a structural unit derived from at least one monomer selected from the group consisting of hexafluoropropylene (HFP), 2,3,3,3-tetrafluoro propylene, and perfluoro(alkyl vinyl ether) (PAVE). The molar ratio of the VdF unit to the structural unit derived from at least one monomer selected from the group consisting of HFP, 2,3,3,3-tetrafluoro propylene, and PAVE is 50/50 to 78/22. The fluororubber composition has a difference δG′ (G′ (1%)-G′ (100%)) of not lower than 120 kPa and not higher than 3,000 kPa, where G′ (1%) denotes a modulus of shearing elasticity at a dynamic strain of 1%, G′ (100%) denotes a modulus of shearing elasticity at a dynamic strain of 100%, and G′ (1%) and G′ (100%) are determined by a dynamic viscoelasticity test.
申请公布号 US2015031822(A1) 申请公布日期 2015.01.29
申请号 US201314380197 申请日期 2013.02.22
申请人 DAIKIN INDUSTRIES, LTD. 发明人 Ota Daisuke;Ueda Akinori;Kadowaki Yuu;Taeda Mayuko;Kitaichi Masanori;Yamamura Kazuhiro;Doi Michiko;Fukuoka Shoji
分类号 C08K3/04 主分类号 C08K3/04
代理机构 代理人
主权项 1. A fluororubber composition comprising: a fluororubber (A); and a carbon black (B), the fluororubber (A) being a vinylidene fluoride-based fluororubber comprising a structural unit derived from vinylidene fluoride (VdF unit) and a structural unit derived from at least one monomer selected from the group consisting of hexafluoropropylene (HFP), 2,3,3,3-tetrafluoro propylene, and perfluoro(alkyl vinyl ether) (PAVE),the molar ratio of the VdF unit to the structural unit derived from at least one monomer selected from the group consisting of HFP, 2,3,3,3-tetrafluoro propylene, and PAVE being 50/50 to 78/22,wherein the fluororubber composition has a difference δG′ (G′ (1%)-G′(100%)) of not lower than 120 kPa and not higher than 3,000 kPa, where G′(1%) denotes a modulus of shearing elasticity at a dynamic strain of 1%, G′(100%) denotes a modulus of shearing elasticity at a dynamic strain of 100%, and G′(1%) and G′(100%) are determined by a dynamic viscoelasticity test carried out on an unvulcanised rubber with a rubber process analyzer (RPA) in a condition that the measurement frequency is 1 Hz and the measurement temperature is 100° C.
地址 Osaka-shi, Osaka JP