摘要 |
The present invention relates to a method for manufacturing a secondary battery, which reduces a pre-aging time during a battery activation process, and secures a waiting time after degassing, thereby improving impregnation properties of the battery. The method for manufacturing a secondary battery of the present invention comprises: a room-temperature aging step of aging a battery injected with an electrolyte at room temperature, a degassing step of removing gas inside the battery aged at room temperature, and having a waiting time after the degassing step. |