摘要 |
<p><P>PROBLEM TO BE SOLVED: To provide a container which is excellent in low-temperature impact resistance and is not whitened in filling at a high temperature. <P>SOLUTION: The container is formed by using a mixed resin composition of polypropylene, linear low-density polyethylene, and low-density polyethylene. <P>COPYRIGHT: (C)2012,JPO&INPIT</p> |