POROUS NOBLE METAL OXIDE NANOPARTICLES, METHOD FOR PREPARING THE SAME AND THEIR USE |
摘要 |
The present invention discloses a method for preparing porous noble metal oxide nanoparticles, comprising the following steps: a) preparing an Olea Europaea fruit extract; b) preparing an Acacia Nilotica extract; c) mixing the Olea Europaea fruit extract and the Acacia Nilotica extract for preparing a mixed extract; d) providing an aqueous solution containing a noble metal compound dissolved therein; e) mixing the mixed extract obtained in step c) and the aqueous solution of step d); f) dropping a solution of sodium chloride to be mixture of step b); d) drying the mixture, in air or by vacuum, and h) calcining at a temperature between 100 to 900° C., to get the porous noble metal oxide nanoparticles; porous noble metal oxide nanoparticles obtained thereby and their use. |
申请公布号 |
US2015219633(A1) |
申请公布日期 |
2015.08.06 |
申请号 |
US201414468485 |
申请日期 |
2014.08.26 |
申请人 |
King Saud University |
发明人 |
HENDI Awatif Ahmed;AWAD Manal A.;EISA Nada E.;ORTASHI Khaled M. |
分类号 |
G01N33/52;C01G7/00 |
主分类号 |
G01N33/52 |
代理机构 |
|
代理人 |
|
主权项 |
1. Method for preparing porous noble metal oxide nanoparticles, comprising the following steps:
a) preparing an Olea Europaea fruit extract b) preparing an Acacia Nilotica extract c) mixing the Olea Europaea fruit extract and the Acacia Nilotica extract for preparing a mixed extract d) providing an aqueous solution containing a noble metal compound dissolved therein, and e) mixing the mixed extract obtained in step c) and the aqueous solution of step d) f) dropping a solution of sodium chloride to the mixture of step e) g) drying the mixture, preferably in air or by vacuum, and h) calcining at a temperature between 100 to 900° C., to get the porous noble metal oxide nanoparticles. |