摘要 |
Melt-blown fiber comprising a terpolymer of propylene, ethylene and a C4 to C10 a-olefin, wherein further said melt blown fiber and/or said terpolymer has/have a melt flow rate MFR25 (230o C) of at least 300 g/10min, the amount of propylene in said terpolymer is at least 90.0 wt.-%, the weight ratio of ethylene and a-olefin within said terpolymer is 1/100 to below 1/1, and the terpolymer has <2,1> regiodefects of below 0.4 mol.-%.10 |