摘要 |
A process for recovering hard material particles which are present in a residue quantity, which is in a free-flowing or pourable form, of a hard metal which has a matrix consisting of a steel, nickel or a nickel alloy, in which the hard material particles are embedded, comprising the following production steps: pouring the residue quantity into an acid bath which contains a strong acid having a pKa value measured at room temperature of <4, adding an oxidant to the acid bath, wherein by adding the oxidant or the acid a redox potential of the acid bath is set which is within a desired range of 300-800 mV, dissolving the matrix of the residue quantity, and depositing of the hard material particles contained in the acid bath after dissolving the matrix. |