发明名称 |
Method for arc welding |
摘要 |
A method for arc welding can control the increase slopes of the short-circuit current and the inflection point of the increase slopes in the welding start period to be smaller than in the steady-state welding period. Thus, the increase slopes of the short-circuit current and the inflection point are made different between the welding start period and the steady-state welding period, thereby reducing sputtering in the welding start period. |
申请公布号 |
US8993926(B2) |
申请公布日期 |
2015.03.31 |
申请号 |
US201113517085 |
申请日期 |
2011.09.28 |
申请人 |
Panasonic Intellectual Property Management Co., Ltd. |
发明人 |
Fujiwara Junji;Kawamoto Atsuhiro;Nakagawa Akira |
分类号 |
B23K9/00;B23K9/09;B23K9/10 |
主分类号 |
B23K9/00 |
代理机构 |
Panasonic Patent Center |
代理人 |
Panasonic Patent Center |
主权项 |
1. A method for arc welding in which welding is performed by alternating a short-circuit state and an arc state using a welding wire as a consumable electrode, the method comprising:
a first short-circuit welding for welding in a welding start period with a first short-circuit current; and a second short-circuit welding for welding in a welding steady period subsequent to the welding start period with a second short-circuit current, wherein: the first short-circuit current has a first increase slope, a second increase slope subsequent to the first increase slope and a first inflection point at which the first short-circuit current changes from the first increase slope to the second increase slope; the second short-circuit current has a third increase slope, a fourth increase slope subsequent to the third increase slope and a second inflection point at which the second short-circuit current changes from the third increase slope to the fourth increase slope; the third increase slope is steeper than the first increase slope; and the fourth increase slope is steeper than the second increase slope. |
地址 |
Osaka JP |