发明名称 |
OPTICAL FILM WITH ADHESIVE LAYER, AND IMAGE DISPLAY DEVICE |
摘要 |
A pressure-sensitive adhesive layer-attached optical film of the present invention comprises an optical film; and a pressure-sensitive adhesive layer and made from an ammonia-containing water-dispersible pressure-sensitive adhesive, wherein the pressure-sensitive adhesive layer has an ammonia content of 10 to 500 μg per 1 g of the pressure-sensitive adhesive layer, and shows a difference of 0 to 500 μg per 1 g of the pressure-sensitive adhesive layer in ammonia content before and after a heat durability test and humidity durability test, and the optical film includes a polarizing film with a degree of polarization of 99.99% or more. The pressure-sensitive adhesive layer-attached optical film has optical properties which are less changeable even in a high-temperature and/or high-humidity environment. |
申请公布号 |
US2014347727(A1) |
申请公布日期 |
2014.11.27 |
申请号 |
US201314368448 |
申请日期 |
2013.01.08 |
申请人 |
NITTO DENKO CORPORATION |
发明人 |
Inui Kunihiro;Ishii Takaaki;Murayama Kazuki;Hosokawa Toshitsugu;Satake Masayuki |
分类号 |
G02B1/10;C09J7/02;G02B5/30 |
主分类号 |
G02B1/10 |
代理机构 |
|
代理人 |
|
主权项 |
1. A pressure-sensitive adhesive layer-attached optical film, comprising:
an optical film; and a pressure-sensitive adhesive layer for an optical film placed on at least one side of the optical film and made from an ammonia-containing water-dispersible pressure-sensitive adhesive, wherein the pressure-sensitive adhesive layer has an ammonia content, measured by attributing to the pressure-sensitive adhesive layer, of 10 to 500 μg per 1 g of the pressure-sensitive adhesive layer, the pressure-sensitive adhesive layer shows a difference of 0 to 500 μg per 1 g of the pressure-sensitive adhesive layer in ammonia content before and after a heat durability test in which the pressure-sensitive adhesive layer is heated at 90° C. for 1,000 hours and also shows a difference of 0 to 500 μg per g of the pressure-sensitive adhesive layer in ammonia content before and after a heat and humidity durability test in which the pressure-sensitive adhesive layer is stored at 60° C. and 95% R.H. for 1,000 hours, and the optical film includes a polarizing film with a degree of polarization of 99.99% or more. |
地址 |
Ibaraki-shi, Osaka JP |