发明名称 ALLOYS WITH LOW COEFFICIENT OF THERMAL EXPANSION AS PDC CATALYSTS AND BINDERS
摘要 A cutting table includes a lattice structure and a catalyst material deposited within voids formed within the lattice structure. The catalyst material is deposited in the voids during a sintering process that forms the lattice structure. The catalyst material facilitates the growth of the lattice structure. The catalyst material has a coefficient of thermal expansion that is less than that of cobalt.
申请公布号 US2014223835(A1) 申请公布日期 2014.08.14
申请号 US201414255740 申请日期 2014.04.17
申请人 Thigpen Gary M.;King William W. 发明人 Thigpen Gary M.;King William W.
分类号 B24D3/10 主分类号 B24D3/10
代理机构 代理人
主权项 1. A cutting table, comprising: a lattice structure forming interstitial spaces therein; and a catalyst material deposited within the interstitial spaces during a sintering process that forms the lattice structure, the catalyst material facilitating the growth of the lattice structure, the catalyst material having a coefficient of thermal expansion that is less than the coefficient of thermal expansion of cobalt.
地址 Houston TX US
您可能感兴趣的专利