摘要 |
A single-crystal silicon pulling silica container including: a transparent silica glass layer in the inner side of the silica container; and an opaque silica glass layer containing gaseous bubbles in the outer side of the silica container, wherein the transparent layer constitutes of a high-OH group layer placed on an inner surface side of the silica container containing the OH group at a concentration of 200 to 2000 ppm by mass and a low-OH group layer having the OH group concentration lower than the high-OH group layer containing Ba at a concentration of 50 to 2000 ppm by mass. Resulting in the silica container used for pulling single-crystal silicon, providing the silica container improves etching corrosion resistance of the container inner surface to silicon melt when the entire inner surface of transparent silica glass of the container is crystallized short after using the container and method for such silica container. |