发明名称
摘要 <p>The present invention is directed to a hybrid process using ion exchange resins in the selective recovery of nickel and cobalt of leaching effluents that is comprised of the steps of processing (1) the laterite ore (M), which is then treated through leaching (2) (either atmospheric or under pressure), considering solutions from the solid-liquid separation step of existing plants already in operation (2) as well, in a way that the downstream process comprises an ion exchange hybrid circuit, wherein the first ion exchange step (3) with resins (Re) exhibits specific selectivity conditions for the removal of iron, aluminum and copper and an increased pH, and the second ion exchange step (4) allows the removal of nickel and cobalt.</p>
申请公布号 JP5282027(B2) 申请公布日期 2013.09.04
申请号 JP20090503374 申请日期 2007.02.02
申请人 发明人
分类号 C22B23/00;B01J49/00;C02F1/42;C22B3/04;C22B3/42 主分类号 C22B23/00
代理机构 代理人
主权项
地址