摘要 |
In the method of cutting steel for machine structural use, steel for machine structural use, in which chemical components contain, by mass %, 0.01% to 1.2% of C, 0.005% to 3.0% of Si, 0.05% to 3.0% of Mn, 0.001% to 0.2% of P, 0.001% to 0.35% of S, 0.002% to 0.035% of N and 0.05% to 1.0% of Al, in a case in which [Al%] and [N%] represent the mass % of Al and N in the steel respectively, [Al%]-(27/14)×[N%]>=0.05% is satisfied, is the other elements are included as necessary, and a balance consisting of Fe and inevitable impurities, is used, and a cutting process is carried out on the steel for machine structural use using water-insoluble cutting oil in which the amount of dissolved oxygen is 4 volume % to 16 volume %.
|