发明名称 Heat-resistant TiAl alloy
摘要 <p>A heat-resistant titanium alloy comprises 43-45 atomic% molybdenum, 0.5-3 atomic% niobium, 0-4.9 atomic% vanadium, chromium, manganese and iron, 0-0.5 atomic% zirconium and hafnium, 0.1-1 atomic% carbon, 0.05-0.2 atomic% boron and 0-1 atomic% silicon, and remaining aluminum and titanium. The composition is selected such that the precipitation of titanium-rich carbide precipitates and solidification of carbon in the mixed crystals of the alloy are eliminated. An independent claim is included for manufacture of the alloy.</p>
申请公布号 EP2620517(A1) 申请公布日期 2013.07.31
申请号 EP20120152427 申请日期 2012.01.25
申请人 MTU AERO ENGINES GMBH 发明人 SMARSLY, WILFRIED, DR.;CLEMENS, HELMUT, PROF.DR.
分类号 C22F1/18;C22C1/04;C22C14/00 主分类号 C22F1/18
代理机构 代理人