摘要 |
<P>PROBLEM TO BE SOLVED: To provide a continuous casting method for high-carbon steel, preventing a side face crack from occurring in a slab. <P>SOLUTION: One or more of the cooling water flow rate q of short-side side members 5a of a mold 5, the immersion depth d of an immersion nozzle, and a continuous casting speed V are adjusted such that a heat removal amount Q per unit time from the short-side side members 5a of the mold 5 becomes a prescribed value Q<SB POS="POST">0</SB>or above. <P>COPYRIGHT: (C)2013,JPO&INPIT |