摘要 |
Provided is a method of producing a porous glass having a high strength by a safe, simple process that does not involve the use of any high-temperature heat treatment or acid treatment step. The method includes: mixing 4 wt % or more to 6.5 wt % or less of sodium oxide, 26 wt % or more to 36 wt % or less of boron oxide, and 60 wt % or more to 68 wt % or less of silicon oxide; heating the mixed materials to melt the materials and cooling the molten materials to obtain a glass body; and a step involving bringing the glass body into contact with water without reheating the glass body to obtain the porous glass.
|