摘要 |
The method for producing a porous positive electrode material for a lithium ion cell of the present invention comprises a preparation step for preparing a starting liquid comprising (I) one or more substances selected from a positive electrode active substance capable of occlusion and release of lithium, production intermediates thereof, and starting materials thereof, wherein the media diameter d50 is no greater than 100% of the median diameter d50 of the following (II), (II) water-dispersible resin microparticles having a median diameter d50 that is between 10 and 400 nm, and an aqueous solvent, and a step for spray drying the starting liquid obtained by the preparation step. The median diameter d50 here is defined as the median diameter d50 in the volume-standard grain size distribution as measured by a laser diffraction/scattering-type distribution meter before preparing the starting liquid. |
申请人 |
MITSUI CHEMICALS, INC.;NAGASAKI UNIVERSITY;MAEKAWA, HIROSHI;NAKAYAMA, NORIO;YOSHIMURA, TOSHIHIRO;SARUYAMA, MASAKI;MORIGUCHI, ISAMU;YAMADA, HIROTOSHI;URITA, KOKI |
发明人 |
MAEKAWA, HIROSHI;NAKAYAMA, NORIO;YOSHIMURA, TOSHIHIRO;SARUYAMA, MASAKI;MORIGUCHI, ISAMU;YAMADA, HIROTOSHI;URITA, KOKI |