发明名称 Infiltration of hard particles with molten liquid binders including melting point reducing constituents, and methods of casting bodies of earth-boring tools
摘要 The present invention relates to compositions and methods for forming a bit body for an earth-boring bit. The bit body may comprise hard particles, wherein the hard particles comprise at least one of carbide, nitride, boride, and oxide and solid solutions thereof, and a binder binding together the hard particles. The binder may comprise at least one metal selected from cobalt, nickel, and iron, and at least one melting point-reducing constituent selected from a transition metal carbide in the range of 30 to 60 weight percent, boron up to 10 weight percent, silicon up to 20 weight percent, chromium up to 20 weight percent, and manganese up to 25 weight percent, wherein the weight percentages are based on the total weight of the binder. In addition, the hard particles may comprise at least one of (i) cast carbide (WC+W2C) particles, (ii) transition metal carbide particles selected from the carbides of titanium, chromium, vanadium, zirconium, hafnium, tantalum, molybdenum, niobium, and tungsten, and (iii) sintered cemented carbide particles.
申请公布号 US8172914(B2) 申请公布日期 2012.05.08
申请号 US20080192292 申请日期 2008.08.15
申请人 MIRCHANDANI PRAKASH K.;EASON JIMMY W.;OAKES JAMES J.;WESTHOFF JAMES C.;COLLINS GABRIEL B.;BAKER HUGHES INCORPORATED;TDY INDUSTRIES, INC. 发明人 MIRCHANDANI PRAKASH K.;EASON JIMMY W.;OAKES JAMES J.;WESTHOFF JAMES C.;COLLINS GABRIEL B.
分类号 C09K3/14;B21K5/02;C22C29/00;C22C29/06;E21B10/46 主分类号 C09K3/14
代理机构 代理人
主权项
地址