发明名称 GROUT AND METHOD FOR MANUFACTURING THE SAME
摘要 <P>PROBLEM TO BE SOLVED: To provide a grout exhibiting a pH in a neutral range (for example, 5.8 to 8.6) during transferring and filling, causing no material separation in water, having good plasticity, and capable of developing a large solidification strength after filling. <P>SOLUTION: The grout contains a sulfate salt (for example, aluminum sulfate) and a magnesium compound (for example, magnesium oxide and a partial hydrate of magnesium oxide). The grout can further contain a thickener (for example, galactomannan) and calcium carbonate. The grout can be prepared by mixing an A material containing a sulfate salt and water (the A material may contain a thickener) with a B material containing a magnesium compound and water (the B material may contain calcium carbonate) in use. <P>COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP2012082306(A) 申请公布日期 2012.04.26
申请号 JP20100228859 申请日期 2010.10.08
申请人 TAIHEIYO CEMENT CORP;TODA CONSTR CO LTD 发明人 MATSUYAMA YUSUKE;MORIYA MASAHIKO;TANAKA TORU;KOBAYASHI OSAMU
分类号 C09K17/02;C04B14/28;C04B24/38;C04B28/00;C09K17/06;C09K17/08;C09K17/32;C09K17/40;C09K103/00;E02D3/12 主分类号 C09K17/02
代理机构 代理人
主权项
地址
您可能感兴趣的专利