摘要 |
An aqueous solution is formed by dissolving a dye made of alizarin and a humectant made of glycerin, and alkalized by dissolving a base (alkaline substance), thereby preparing a detector solution (101) in which the content of the humectant is about 20 wt %. An impregnated carrier (104) impregnated with the detector solution (101) is formed by dipping for 30 sec a sheet-like carrier (103) made of cellulose filter paper in the detector solution (101) so that the carrier (103) is impregnated with the detector solution (101). The impregnated carrier (104) is pulled up from the detector solution (101), and dried in dry nitrogen by evaporating a solvent such as water contained in the impregnated carrier (104), thereby forming an ozone detecting device (105).
|