发明名称 |
METHOD FOR PRODUCING FIBER-REINFORCED COMPOSITE MATERIALS FROM POLYAMIDE 6 AND COPOLYAMIDES MADE OF POLYAMIDE 6 AND POLYAMIDE 12 |
摘要 |
The present invention relates to a method for producing fiber-reinforced composite materials, by saturating a plurality of continuous filaments or woven fabrics, optionally together with reinforcement materials, containing caprolactam and other starting materials for polyamide 6, or other starting materials for copolymers of the caprolactam, passing the materials through at temperatures between 70 and 100ºC, and anionically polymerizing them at temperatures between 100 and 190ºC, and optionally re-polymerizing them at temperatures between 90 and 170ºC. |
申请公布号 |
WO2011003900(A2) |
申请公布日期 |
2011.01.13 |
申请号 |
WO2010EP59628 |
申请日期 |
2010.07.06 |
申请人 |
BASF SE;SCHERZER, DIETRICH;KORY, GAD;WEBER, MARTIN |
发明人 |
SCHERZER, DIETRICH;KORY, GAD;WEBER, MARTIN |
分类号 |
B29B15/12 |
主分类号 |
B29B15/12 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|