INCREASING THE STRENGTH OF IRIDIUM, RHODIUM, AND ALLOYS THEREOF |
摘要 |
The addition of 0.5 to 30 ppm boron and 0.5 to 20 ppm calcium to iridium and the Zr- and Hf-free alloys thereof and rhodium and the Zr- and Hf-free alloys thereof surprisingly increases the creep rupture strength at high temperatures, in particular around 1,800° C.
|