发明名称 METHOD OF MAKING SILICA SORBENT
摘要 FIELD: chemistry. ^ SUBSTANCE: invention relates to chemistry and can be used to make silica sorbent. A 30% sodium silicate solution is obtained with modulus 2.8-3.7 in demineralised water at room temperature. Aqueous sulphuric acid solution is also obtained at room temperature by adding sulphuric acid with density of 1.835 g/cm3 to dimineralised water. A hot sodium silicate solution in demineralised water is obtained through preliminary pouring demineralised water into a reactor while stirring and heating to 80-100C and addition of a 30% sodium silicate solution with modulus 2.8-3.7 prepared before hand and maintaining this temperature. Further, sodium silicate solution in demineralised water at room temperature and sulphuric acid solution at room temperature are simultaneously added to the reactor containing hot sodium silicate solution in demineralised water. Sulphuric acid is added in order to attain pH value of 4.5. Filtration, drying, crushing and classification are then carried out. ^ EFFECT: invention enables to obtain sorbent with a fine-grained structure with uniform particle size.
申请公布号 RU2391292(C1) 申请公布日期 2010.06.10
申请号 RU20090123260 申请日期 2009.06.19
申请人 OBSHCHESTVO S OGRANICHENNOJ OTVETSTVENNOST'JU "SINTETICHESKIE KREMNEZEMY" 发明人 LOS' SVJATOSLAV LEONIDOVICH
分类号 C01B33/143 主分类号 C01B33/143
代理机构 代理人
主权项
地址