A method of producing a building material using environment-friendly loess includes preparing an environment-friendly composition by mixing 10˜90 parts by weight of at least one selected from among loess, kaolin, clay and grayish blue powdered soil, 3˜50 parts by weight of a resin coating agent, 0.1˜25 parts by weight of an inorganic pigment, and 1˜60 parts by weight of water; and molding the environment-friendly composition at 10 second˜20 minute intervals by introducing it into a molding machine having a temperature of 50˜550° C. and an internal pressure of 1˜20 kg/cm2. A method of producing a container using environment-friendly loess includes preparing an environment-friendly composition by mixing 10˜90 parts by weight of at least one selected from among loess, kaolin, clay and grayish blue powdered soil, 3˜50 parts by weight of a resin coating agent, 0.1˜25 parts by weight of an inorganic pigment, and 1˜60 parts by weight of water; and molding the environment-friendly composition at 10 second˜20 minute intervals by introducing it into a molding machine having a temperature of 50˜450° C. and an internal pressure of 1˜10 kg/cm2.
|