发明名称 METHOD FOR MANUFACTURING RARE EARTH MAGNET
摘要 <P>PROBLEM TO BE SOLVED: To provide a method for increasing a coercive force by carrying out thermal dispersion treatment in a prescribed atmosphere and temperature and a time after forming a film on the surface of a magnet piece by application. <P>SOLUTION: In this method for manufacturing a rare earth permanent magnet materials, the surface of a rear earth sintered permanent magnet configured of an alloy or inter-metal compound phase with an R<SP>1</SP>-Fe-B system composition (R<SP>1</SP>is one or two elements selected from Nd and Pr) as a main body is covered b or contacts with hypoxia quantity rare earth oxide powder shown by a composition formula R<SP>2</SP>O<SB>x</SB>(R<SP>2</SP>is one or two elements selected from Dy or Tb, x<1.0) obtained by reducing R<SP>2</SP><SB>2</SB>C<SB>3</SB>or R<SP>2</SP>C<SB>2</SB>as the rare earth carbide of R<SP>2</SP>metal with at least one type of high boiling point active metal selected from the group of Ti, Zr, Hf, Mo, Nb, Ta, V, or W, and the thermal dispersion of the R<SP>2</SP>of the R<SP>2</SP>O<SB>x</SB>is carried out from the surface of the magnet. <P>COPYRIGHT: (C)2009,JPO&INPIT
申请公布号 JP2009194262(A) 申请公布日期 2009.08.27
申请号 JP20080035403 申请日期 2008.02.17
申请人 OSAKA UNIV 发明人 MACHIDA KENICHI;ITO MASAHIRO;NISHIMOTO HIROMU;RI TOKUZEN
分类号 H01F41/02;B22F3/24;C22C38/00;H01F1/053 主分类号 H01F41/02
代理机构 代理人
主权项
地址