摘要 |
<p>Mixture for construction of a pulp mixture intended as a base to manufacture prefabricators resp. thermal insulation materials with using of waste, consisting of at least 5% of volume of cellulose mixture and a maximum of 95% of cement with sand volume and industrial dry matter with the benefit of 10% of volume mixture of cellulose and 90% of cement with sand volume and industrial dry mass with the benefit of 90% of volume mixture of cellulose and 10% of cement with sand volume and industrial dry mass, while a mixture of cellulose consists of 100% of volume of cellulose fibers or recycled paper, or at least 30% of volume of cellulose fibers or recycled paper, with the addition of 5 to 10% of volume of water glass and / or 2 to 15% of volume of natural resins and / or 5 to 25% of volume of kaolin and / or 5 to 20% of chalk volume.</p> |