摘要 |
The present invention is directed to a golf ball having at least one layer formed from a moisture resistant composition having a moisture vapor transmission rate of 12.5 g.mil/100 in<SUP>2</SUP>/day or less, a flexural modulus of from 50 kpsi to 70 kpsi, and comprising a highly neutralized acid polymer, wherein the highly neutralized acid polymer is produced by a process comprising contacting the acid polymer with a sufficient amount of a lithium-based cation source, in the presence of a melt flow modifier, to increase the level of neutralization of the copolymer to at least 70%. Golf balls of the present invention include one-piece, two-piece, multi-layer, and wound golf balls. The composition may be present in any one or more of a core layer, a cover layer, or an intermediate layer. |