发明名称 STEEL MAKING METHOD
摘要 FIELD: ferrous metallurgy; treatment of steel in steel-teeming ladle. ^ SUBSTANCE: proposed method includes tapping of melt from converter to ladle, delivery of deoxidizers, alloying and slag-forming materials in the course of tapping and blowing the melt in ladle with neutral gas. After filling of ladle, aluminum is introduced in two portions in melt in form of rods; consumption of aluminum in first portion is set by the following dependence: M1=0.1[0]/K1+1000(0.015-0.050)/K2; then, melt is blown with neutral gas at flow rate of 0.001-0.007 m3/(t.min) during 2-6 minutes, after which second portion of aluminum is introduced into melt at consumption determined from the following dependence: M2=(0.1-0.7)M1; then, melt is blown with neutral gas at flow rate of 0.0005-0.0055 m3/(t.min) during 2-6 min. ^ EFFECT: reduction of consumption of alumo-containing materials; reduced content of oxide inclusions in metal. ^ 1 tbl, 1 ex
申请公布号 RU2290447(C2) 申请公布日期 2006.12.27
申请号 RU20050108948 申请日期 2005.03.28
申请人 OTKRYTOE AKTSIONERNOE OBSHCHESTVO "NOVOLIPETSKIJ METALLURGICHESKIJ KOMBINAT" (OAO "NLMK") 发明人 SUKHANOV JURIJ FEDOROVICH;KHREBIN VALERIJ NIKOLAEVICH;DAGMAN ALEKSEJ IGOR'EVICH;LEBEDEV VLADIMIR IL'ICH
分类号 C21C7/06;C21C7/076 主分类号 C21C7/06
代理机构 代理人
主权项
地址