发明名称 |
PROCESS FOR PRODUCING POWDERY LINEAR POLYMER HAVING IMPROVED POWDER PROPERTIES |
摘要 |
A powdery linear polymer having a narrow particle size distribution with little dusting and excellent in anti-blocking property is recovered from a latex of a linear polymer containing a large proportion (35-75 wt. %) of soft polymer (S) component through a two-step coagulation process including a first (moderate coagulation) step causing 70-98 wt. % of the coagulation. The linear polymer in the latex has a multilayer structure comprising a linear polymer (S) having a glass transition temperature below 40° C. and a linear polymer (H) having a higher glass transition temperature disposed in totally at least two layers and containing 35-75 wt. %, as a whole, of the linear polymer (S) with the proviso that the linear polymer (S) cannot be contained in excess of 30 wt. % in an outermost layer of the multilayer structure. |
申请公布号 |
EP1436333(A4) |
申请公布日期 |
2006.03.22 |
申请号 |
EP20020762882 |
申请日期 |
2002.08.28 |
申请人 |
ROHM AND HAAS COMPANY |
发明人 |
SUZUKI, YASUHIRO;HIGUCHI, ATSUHIRO |
分类号 |
C08F6/22;C08F257/02;C08F265/04;C08F285/00;C08F291/00;C08L51/00;(IPC1-7):C08F6/22 |
主分类号 |
C08F6/22 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|