Method for producing hydroxyl-modified ethylene-alpha-olefin copolymer |
摘要 |
A hydroxyl-modified ethylene-alpha-olefin copolymer with excellent coating properties and adhesion properties are produced by heating a mixture containing 100 parts by weight of an ethylene-alpha-olefin copolymer and 0.1 to 20 parts by weight of a peroxide having a hydroperoxy group. The heating temperature is adjusted within a range from the 10-hour half-life temperature to the 1-minute half-life temperature of the peroxide.
|