摘要 |
PROBLEM TO BE SOLVED: To provide a polyarylene sulfide resin molded article having a good surface state which can be molded at a significantly high crystallization speed without impairing heat resistance, mechanical properties, chemical resistance, dimensional stability and flame retardancy of polyarylene sulfide resins. SOLUTION: The resin composition comprises (A) 100 pts. wt. polyarylene sulfide resin, (B) 0.1-10 pts. wt. aromatic phosphate of a specific structure, and (C) 3-35 pts. wt. polyphenylene oxide resin. COPYRIGHT: (C)2005,JPO&NCIPI
|