发明名称 CONTINUOUS CASTING METHOD OF HIGH-TITANIUM-CONTAINED STEEL
摘要 PROBLEM TO BE SOLVED: To provide a continuous casting method of high-titanium-containing steel which makes a cast steel slab free from any surface defect and enables the high-titanium-containing steel slab to be rolled without care. SOLUTION: In the continuous casting of high-titanium-containing steel containing 0.1-1.0 mass% Ti, the angleθof the delivery hole of an immersion nozzle 1 is within a range between 2 and 8 degrees upward, the immersion depth H of the immersion nozzle is within a range between 80 and 130 mm, and the consumption of molding powder 11 is within a range between 0.3-0.6 kg/m×min. These casting conditions prevent a longitudinal crack and a slag residue, and can produce the cast steel slab excellent in surface properties which can be rolled without care. COPYRIGHT: (C)2005,JPO&NCIPI
申请公布号 JP2005224852(A) 申请公布日期 2005.08.25
申请号 JP20040038322 申请日期 2004.02.16
申请人 JFE STEEL KK 发明人 FUJITA HIROKI;ISHIGE TOSHIAKI;HATORI SATOSHI
分类号 B22D11/00;B22D11/10;B22D11/108;C22C38/00;C22C38/14;(IPC1-7):B22D11/00 主分类号 B22D11/00
代理机构 代理人
主权项
地址