发明名称 MANUFACTURING METHOD OF NONAQUEOUS ELECTROLYTIC SOLUTION BATTERY
摘要 PROBLEM TO BE SOLVED: To provide a manufacturing method of a nonaqueous electrolytic solution battery in which the nonaqueous electrolytic solution is supplied effectively in a short time in the manufacturing method of the battery in which electrolytic solution is supplied after the group of electrode plates in a state that a positive electrode plate and a negative electrode plate are insulated via a separator is housed in a battery can, and a nonaqueous electrolytic solution battery superior in charging and discharging cycle characteristics. SOLUTION: In the state that the battery can in which the group of electrode plates is housed and the electrolytic solution are warmed, the cycles of normal pressure state and reduced pressure state are repeated at least twice, and the electrolytic solution is supplied separately. As for the reduced pressure state, it is preferable not to exceed the pressure value of the previous reduced pressure state for each cycle, and the pressure of the reduced pressure state is preferably between 40 kPa and 80 kPa, and the warming temperature is preferably between 40°C and 100°C. COPYRIGHT: (C)2004,JPO&NCIPI
申请公布号 JP2004241222(A) 申请公布日期 2004.08.26
申请号 JP20030028037 申请日期 2003.02.05
申请人 MATSUSHITA ELECTRIC IND CO LTD 发明人 HOTEHAMA KENICHI;YOKOYAMA TAKASHI
分类号 H01M2/36;H01M10/05;H01M10/0566;H01M10/058;(IPC1-7):H01M10/40 主分类号 H01M2/36
代理机构 代理人
主权项
地址