摘要 |
PROBLEM TO BE SOLVED: To provide a welding wire which can maintain a stable feeding performance even in such critical working conditions that the feeding speed of the welding wire increases or the temperature of the welding wire increases as is the case with the gas shielded arc welding under a high heat input and high interpass temperature. SOLUTION: The steel wire material of the welding wire comprises C:0.005-0.09 mass%, Si:0.50-1.2 mass%, Mn:1.50-2.2 mass%, Ti:0.15-0.30 mass%, B:0.0005-0.0035 mass%, Cu:≤0.50 mass%, S:0.005-0.025 mass% and the balance Fe with unavoidable impurities. The surface of the welding wire is covered by a solid lubricant layer of 0.2-1.0 g per the steel wire material of 10 kg, and the surface of the solid lubricant layer is coated with a lubricant of 0.2-1.8 g per the steel wire material of 10 kg. COPYRIGHT: (C)2004,JPO&NCIPI
|