发明名称 PREFORM, PROCESS FOR PRODUCING THE SAME, AND BIAXIALLY STRETCHED CONTAINER OBTAINED FROM THE PREFORM
摘要 <p>A preform and a container formed from the preform by stretch molding. The preform has at least a layer comprising a polyester resin and has been formed by compression molding. The time required for the layer comprising a polyester resin to come to have a maximum value of the quantity of heat of isothermal crystallization at 210°C is 300 seconds or longer. The resin is hence inhibited from suffering pyrolysis during molding for producing the preform. The preform is effectively inhibited from suffering a decrease in intrinsic viscosity or generating acetaldehyde. A biaxially stretched container excellent in mechanical strength and flavor retention can be provided.</p>
申请公布号 WO2004039559(A1) 申请公布日期 2004.05.13
申请号 WO2003JP13549 申请日期 2003.10.23
申请人 TOYO SEIKAN KAISHA, LTD.;KIKUCHI, JUN;KOMATSU, IKUO 发明人 KIKUCHI, JUN;KOMATSU, IKUO
分类号 B29B11/12;B29C43/08;B29C43/42;B29C49/00;B29C49/02;B29C49/08;B29C49/22;(IPC1-7):B29C49/02 主分类号 B29B11/12
代理机构 代理人
主权项
地址