摘要 |
PROBLEM TO BE SOLVED: To provide a stainless steel strip having excellent shape fixability in which the defects of shape such as springback and twist appearing in a formed product can be reduced by using an inexpensive material having a low Ni content, and to provide a production method therefor. SOLUTION: The stainless steel strip is obtained by subjecting ferritic stainless steel having a composition containing, by mass, <=0.10% C, <=1.0% Si, <=1.0% Mn, <=0.050% P, <=0.020% S, <=2.0% Ni, 8.0 to 22.0% Cr and <=0.05% N, and, if required, further containing one or more kinds selected from <=0.10% Al, <=1.0% Mo, <=1.0% Cu, 0.01 to 0.50% Ti, 0.01 to 0.50% Nb, 0.01 to 0.30% V, 0.01 to 0.30% Zr and 0.0010 to 0.0100% B, and the balance Fe with inevitable impurities to hot rolling, and thereafter subjecting the steel sheet to batch annealing at 700 to 880 deg.C for 1 to 24 hrs.
|