发明名称 |
METHOD FOR PRODUCING AMORPHOUS RIBON FOR NANO- CRYSTALLIZED MATERIAL AND METHOD FOR MANUFACTURING NANO-CRYSTALLIZED SOFT MAGNETIC MATERIAL USING THIS RIBON |
摘要 |
PROBLEM TO BE SOLVED: To provide a production method of an Fe base amorphous ribon with which a nano-crystallized material excellent in magnetic characteristic can be obtained, and a manufacturing method of a nano-crystallized soft magnetic material using this amorphous ribon. SOLUTION: This amorphous ribon for nano-crystallized material is produced by pouring molten metal composed of <=10 mol% B and <=15 mol% one or more elements in 4A, 5A and 6A groups in the periodic table of elements and the balance substantially Fe into a moving cooling body while introducing gas having >=32 J/mol.K specific heat at constant pressure at 30 deg.C toward this molten metal. The nano-crystallized soft magnetic material having <=100 nm average crystallized grain diameter can be obtained by applying the heat treatment to this ribon at not lower than the crystallized temperature. |
申请公布号 |
JP2001300697(A) |
申请公布日期 |
2001.10.30 |
申请号 |
JP20000124840 |
申请日期 |
2000.04.25 |
申请人 |
HITACHI METALS LTD |
发明人 |
SUNAKAWA ATSUSHI;BIZEN YOSHIO;YOSHIZAWA KATSUTO |
分类号 |
B22D11/06;C22C1/00;C22C45/02;H01F1/153 |
主分类号 |
B22D11/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|