摘要 |
electronic engineering; manufacture of gas panels. SUBSTANCE: thin and transparent coating noted for highly developed structure is formed due to using high-melting filler powder in the amount of 2-6 parts by weight and organic binder in the amount of 94-98 parts by weight; specific surface area of high-melting filler powder is 10 000-30 000 sq.cm/g. Oxides of following metals may be used as high-melting fillers: magnesium, yttrium, lanthanum, and aluminum; 4-8% solution of ethyl cellulose in turpentine oil with 3-7% of dibutyl phthalate may be used as organic binder. EFFECT: improved quality of coating produced by means of proposed compound. 3 cl
|